Anhui Jwell Precision Mold Co., Ltd.

Several critical aspects must be carefully controlled when using this production line. Temperature control is the lifeline of quality. The temperature from the feed section to the die connection of the barrel must increase gradually. The die temperature should be slightly higher than the barrel by 5 to 10 degrees Celsius, and both ends should also be higher than the temperature inside the die to ensure uniform and stable melt flow. The die lip gap must be precisely equal to or slightly smaller than the target sheet thickness, and the die lip straightness must be controlled within plus or minus 0.002 millimeters per meter to ensure consistent sheet thickness. In the three-roller calendering system, the feed roller temperature should be slightly higher and the discharge roller temperature slightly lower, with roller surface roughness not exceeding 0.2 micrometers. Residual material must be cleaned with copper blades rather than hard steel tools to avoid scratching the roller surface. The three-roller operating speed should be slightly higher than the extrusion speed and controlled within a 10 percent speed difference; running too fast or too slow will both cause thickness deviations. In addition, the moisture content of PET raw materials must be strictly controlled below 0.005 percent, and crystallization treatment must be completed before production at temperatures below 149 degrees Celsius to prevent hydrolytic degradation that leads to reduced impact strength. The equipment must be regularly inspected for screw concentricity, gear meshing precision, and bearing wear conditions, with molds and blades and other wear parts replaced in a timely manner to ensure long-term stable operation and continuous production of high-quality seedling tray sheets.